20/02/2026

4:1 Heat shrink tubing in straight 1.2m lengths
Art.-No. 317-00011 | TG40 8/1.65-PO-X-CL

Copied
  • Thin-walled (time, cost and weight saving)
  • 4:1 shrink ratio (for challenging geometries, higher surface pressure)
  • With thermoplastic (hot-melt) adhesive
  • Continous operating temperature up to +125°C
  • Peak temperature up to 225°C/4h (heat shock test)
  • Self-extinguishing (BK) / Halogen-free (CL)
  • Resistant against acids, alkalis, oils and fuels
Application TG40 is a semi-rigid polyolefin heat shrink tubing with thermoplastic (hot-melt) adhesive designed to insulate, seal and protect wire bundles, connectors, terminals and in-line splices in automotive wire harnesses and electronic assemblies.
Behaviour At Low Temperature not cracking
Behaviour at Heat Shock not cracking, not dripping, not fluid
Behaviour at low Temperature test method UL 224
Color Clear (CL)
Elongation At Heat Aging 220%
Heat Aging Test 168h/158°C
Heat Aging test method ASTM D2671
Heat Shock Test 4h/225°C
Minimum Tensile Strength At Heat Aging 12MPa
PART DESCRIPTION TG40 8/1.65-PO-X-CL
Packaging Type pcs.
Part No. 317-00011
Product family Insulation
Type TG40 8/1.65
For Object Outside Diameter 2.92-6.73 mm
Length (metric) 1.22m
Longitudinal Change After Shrinkage +/-10% max
Printable No
Recovered Diameter (metric) 1.65mm
Shrink Ratio 4:1
Supplied Diameter (metric) 8.0mm
Volume Resistance 10¹⁴ Ω cm
Wall Thickness (metric) 1.52mm
Adhesive Hot melt adhesive
Dielectric Strength 19.5kV/mm
Dielectric Strength test method IEC 60243
Elongation at break (min.) 500%
Elongation at break test method ASTM D2671
Halogen Free Yes
Material PO-X
Material Polyolefin, cross-linked (PO-X)
Min. Shrink Temperature +230 °F (+110 °C)
Operating Temperature -67°F to +257°F (-55°C to +125°C)
REACH Conformity Yes
ROHS compliant Yes
Test Method Tensile Strength ASTM D2671
Volume Resistance test method ASTM D2671
Packaging 1 - Weight (kg) 0.025001kg
Pkg. Qty. 1.22m